ELECTRICAL IGNITER CABLE
Listed below are suggested high resistance wires for use in making electrical firing systems. General recommendations are that the wires used for ignition need a to have a resistance range of 650 to 875 ohms/cmf, with the higher end of the range being the best suited. Melt point of the wire needs to be in the range of 1100-1500° C.
| Composition | Resistance |
Melt Point (°C) |
Also Known As | |
| EvanOhm | 75% Nickel, 20% Chrome 2.5% Aluminum 1.7% Copper |
800 | 1400° C | Alloy 800, Stablohm 800, Nikrothal LX, Chromel R, Karma, Evanohm, Evenohm, Evanohm R, Evenohm R, HAI-431, Moleculoy, 800 Alloy. |
| NiCr 80 | 80% Nickel |
650 | 1200° C | Chromel A, Nikrothal 80, N8, Nichrome V, HAI-NiCr 80, Tophet A, Resistohm 80, Cronix 80, Protoloy, Nikrothal 8, Alloy A, MWS-650, Stablohm 650 |
NiCr 60 |
60% Nickel |
675 | 1390° C | Chromel C, Nikrothal 60, N6, HAI-NiCr 60, Tophet C, Resistohm 60, Cronifer II, Electroloy, Nichrome, Alloy C, Nikrothal 6, MWS-675, Stablohm 675 |
| Alloy 815 | 22% Chrome 73.2% Iron 4.8% Aluminum |
815 | 1500° C | Kanthal D, Kanthal, Alloy 815, Alchrome DK, Alferon 901, Resistohm 135, Aluchrom 5, Stablohm 812 |
| Alloy 837 | 22% Chrome 72.7% Iron 5.3% Aluminum |
836 | 1500° C | Kanthal AF, Resistohm Y, Aluchrom Y, Alloy 837 |
| Alloy 875 | 22% Chrome 72.2% Iron 5.8% Aluminum |
875 | 1500° C | Kanthal A1, Kanthal, Alloy 875, Resistohm 145, Aluchrom 0, Alchrome 875, MWS-875, Stablohm 875 |